Product Name
4J33 Alloy Powder
Category
Precision Alloy Powders
Description
The linear expansion coefficient of 4J33 alloy is close to that of 95% Al2O3 ceramics in the temperature range of -60 °C to 600 °C.
Application
Selective laser melting (SLM)
Feedstock for additive manufacturing processes such as electron beam melting (EBM)
Additives for special applications
Feature
High powder sphericity, smooth surface, high material purity, low oxygen content, uniform particle size distribution, good flowability, high apparent density, high vibration density
Melting Temperature
1450 °C
Packing Type
As per customer requirement
Particle Size
5-15 μm, 15-45 μm, 15-53 μm, 45-105 μm, 45-150 μm, or customizable
Processing Method
Atomization
Storage Conditions
4J33 alloy powder should be well sealed and stored in a cool and dry place, avoiding direct light.